Moisture in the element
01
Concrete gains strength through hydration, which requires water. Where the surface dries before hydration is sufficiently advanced, the outer layer gains less strength than the core.

Precast Concrete · Process
Curing is the process of keeping concrete at a suitable moisture content and temperature while it gains strength. It begins as soon as placing finishes and continues for days, and it determines whether the material reaches the properties the design relied on.
It is a process rather than a test, and that is why it is easy to under-manage. Nothing visible happens while it is going wrong, and the consequences appear days later as cracking, low strength results or a surface that fails its finish class.
Zabidou measures the geometry and surface of every element as it comes off the line, which is where those consequences first become visible.
Zabidou in production today
QLD + VIC
Operating in factories across Queensland and Victoria today.
100%
Inspection coverage on finished items as they come off the line.
Silver
Associate Member, Australian Steel Institute.
Bronze
Member, National Precast Association Australia.
Curing manages three conditions at once. Where any one of them moves outside its range the element can be affected, and the three interact rather than acting independently.
01
Concrete gains strength through hydration, which requires water. Where the surface dries before hydration is sufficiently advanced, the outer layer gains less strength than the core.
02
Rate of strength gain rises with temperature, but heat applied too quickly, or lost too quickly, produces internal stress. Steam curing in precast is a controlled version of this, not an exception to it.
03
Stripping early frees the bed, and it also applies handling loads to an element that has not reached the strength assumed. Most demould damage is a curing decision rather than a handling error.
A curing failure is rarely identified as one. It surfaces as something else, days or weeks later, and by then the connection back to the cause has usually been lost.
01
A cylinder returns below specification. The mix was correct and the placing was correct, and the deficit traces back to conditions during the days after casting.
02
Plastic shrinkage and early thermal cracking both originate in the hours and days after placing. The crack is visible; the condition that caused it was not.
03
Edges spall, corners break away and faces mark. The damage is logged against handling, and the element was stripped before it was ready.
The expensive part of a curing problem is that it is discovered after the element is finished, which puts every option into the rework column. What Zabidou changes is how early that discovery happens.
An element with a curing-related defect cannot be corrected at the point the problem occurred, because by then the concrete has hardened. The options are repair to an agreed standard, a concession, or scrap and recast.
Each of those carries the full cost of the element plus the delay to whatever it was scheduled for, and a recast consumes bed time that was already allocated to the next pour.
What inline measurement contributes here is narrower than the whole problem, and it is worth being precise about it. Zabidou measures geometry and surface condition on every element as it comes off the line, so dimensional and surface consequences are detected immediately and attributed to the right batch and bed.
For the plant, that means a curing problem is attributed to the right batch and bed while it is still one repair, rather than after a week of pours has gone the same way. The same check runs on a precast concrete bed and on a steel fabrication line.
It does not measure strength, moisture or internal temperature, and no camera does.
A curing problem usually shows up as a low strength result or as cracking. It is worth separating from compaction defects such as honeycombing, and cracking matters most where it reaches the concrete cover protecting the reinforcement.
Five checks run on every element as it comes off the line, and together they catch the dimensional and surface consequences of a curing problem on the first affected element rather than the thirtieth.
Complete 3D measurement and verification of as-built output against a Golden Sample or design intent, for full dimensional compliance without stopping the line.
Automated, real-time verification that components are correctly positioned before and during production, while the mould is still open or the section is still in the jig.
Inline detection of surface defects, voids and irregularities at industrial speed, fully automated and without manual inspection.
Precise measurement and verification of critical dimensions against a Golden Sample or the drawings, inline, in real time, at scale.
Manufactured-unit centric digital provenance that automatically delivers the full audit history operations, financiers and customers demand.
The same underlying cause produces very different outcomes depending on how long it goes unnoticed.
| At demould | At dispatch | After delivery | |
|---|---|---|---|
| What is seen | Edge damage or surface marking on one element. | A pattern across several elements. | A rejected element on site. |
| What it costs | Repair or recast of that element. | Repair or recast of a batch, plus the hold. | The element, the delivery, and the site's sequence. |
| Can the cause be traced | Usually, the bed and batch are known. | With effort, if records are good. | Rarely with confidence, weeks later. |
| What stops a recurrence | Adjust the curing regime that shift. | Review the regime and the strip criteria. | A corrective action and a customer conversation. |


Curing is the process of maintaining suitable moisture and temperature in concrete while it gains strength. It begins when placing finishes and continues for days, and it determines whether the material develops the properties the design assumed.
It is distinct from setting, which is the initial stiffening of the mix, and from drying, which is moisture leaving the element afterwards.
The period depends on the mix, the ambient conditions, the element and the strength required before the next operation. Precast production commonly uses accelerated methods to reach strip strength in hours rather than days.
The practical answer on any given job comes from the specification and the strip criteria rather than from a general rule.
The surface layer gains less strength than the core, which shows up as reduced durability, plastic shrinkage or early thermal cracking, surface defects and in some cases strength results below specification.
The damage is permanent. Curing cannot be applied retrospectively once the concrete has hardened.
Curing keeps water in the concrete so hydration can continue. Drying is water leaving the element after hydration is sufficiently advanced.
Treating the two as the same thing is the usual reason curing gets cut short, since an element that looks dry on the surface may still be curing internally.
Not directly. Cameras and lasers measure geometry and surface condition, not strength, moisture or internal temperature.
What inline measurement does is detect the dimensional and surface consequences on every element as it comes off the line, which makes a developing pattern visible early and ties it to a specific bed and batch.